ERNiCrCoMo-1 welding wire is used for welding of low carbon nickel cobalt chromium molybdenum alloy (UNS N06617) and steel surface surfacing. It can also be used for the welding of dissimilar high-temperature alloys (which have high-temperature strength and oxidation resistance at around 1150°C) and cast high-nickel alloys.
ERNiCrCoMo-1 welding wire is used for welding of low carbon nickel cobalt chromium molybdenum alloy (UNS N06617) and steel surface surfacing. It can also be used for the welding of dissimilar high-temperature alloys (which have high-temperature strength and oxidation resistance at around 1150°C) and cast high-nickel alloys.
Ni≥44.0%
Cr:20%~24%
Co:10.0%~15.0%
Mo:8.0%~10.0%
Fe≤3.0%
Al:0.8%~1.5%
Mn≤1.0%
Si≤1.0%
Ti≤0.6%
Cu≤0.5%
C:0.05%~0.15%
P≤0.02%
S≤0.015%